A. Thermosetting polymers
B. High carbon steels
C. Brasses
D. Borosilicate glasses
Correct Answer: Brasses ✔
Last Updated: February 11, 2019
A. Thermosetting polymers
B. High carbon steels
C. Brasses
D. Borosilicate glasses
Correct Answer: Brasses ✔