In panel test for spalling resistance, the average face temperature of panel assembly is maintained at _____________ °C for 24 hours?
Related MCQs
Fireclay bricks is not used for lining the__________?
Fireclay refractories__________?
Silica bricks are never used for lining the__________?
Refractory bricks having lower porosity have __________?
Ceramic recuperators used for waste heat recovery from high temperature flue gas going out of the furnace is made of __________?
Pure oxide refractories are generally monocrystalline in nature and are self bonded __________ bricks are generally used as moderator in nuclear reactors?
Quartz is__________?
With increase in the porosity, thermal spalling resistance of fireclay brick__________?
Refractoriness/fusion points of ‘Superduty’ refractories is __________ °C?
Capacity of a refractory brick to withstand-sudden changes in temperature is denoted by the property called__________?
In panel test for spalling resistance, the average face temperature of panel assembly is maintained at _____________ °C for 24 hours?
A. 700
B. 1000
C. 1600
D. 2000
Correct Answer:
1600
✔